Correlation between low corrosion resistance and osteosarcoma

Correlation between low corrosion resistance and osteosarcoma

Sprecher CM, Boudrieau RJ, Suter T, Keating JH, McCarthy RJ, Gueorguiev B, Richards G, Milz S

Objective: Peri-implant osteosarcoma (OSA) occurrence was found in dogs treated with the Slocum cast stainless steel tibial plateau leveling osteotomy (TPLO) plate. Recently, it was assumed that the metallurgical inhomogeneity of the plate surface, or the reduced corrosion resistance of the cast stainless steel material, were related to OSA occurrence. Therefore, the aim of the current study was to investigate the corrosion behavior of TPLO plate surfaces from animals with and without OSA.

Method: Eighteen retrieved 316L cast stainless steel Slocum TPLO plates, 9 from dogs with (CwOS) and 9 from dogs without peri-implant osteosarcoma (CnOS) were investigated. Three retrieved forged stainless steel TPLO plates (Synthes) from dogs without osteosarcoma (FnOS) represented a different manufacturing process. On all plates, visual inspections with a stereomicroscope and local micro electrochemical corrosion measurements were performed on plastic deformed surface areas in 1M NaCl on various spots (d=0.1mm) and corrosion resistance factors (CRF) were calculated. To assess the metallurgical inhomogeneity, nine randomly positioned corrosion measurements were performed on one plate of each group. The Mann-Whitney U Test was used for statistical analysis.

Results and conclusion: The time in-situ was comparable for both cast implant groups (CwOS 59±19 months vs. CnOS 52±14 months) and was shorter for FnOS (35±5 months). Microscopic inspections on the cast groups showed rough surfaces, residues and signs of local corrosion attacks. Furthermore, local notches and more severe tool marks were found next to the contoured regions of the plate. On the forged plates only few marks, but no residues or microscopic signs of corrosion could be detected. The CRF values determined on different surface spots showed a wide variation for the cast plates and a small bandwidth in forged plates; the differences between groups were significant (p<0.001). Repeated measurements on one plate of each group showed a significantly higher ion production for CwOS than for CnOS (p=0.008) or FnOS (p<0.001).

The local micro electrochemical corrosion measurements showed no clear difference between local corrosion behaviors of the two groups of cast plates due to a large standard deviation. The ion measurements clearly show a significant increase of ion release for the OSA group, which resembles the metallurgical inhomogeneity of the plate surface. Both corrosion and metal ion release result in chronic inflammation in the tissues with oncogenic effects; furthermore, direct toxic effects of these ions may also contribute to a foreign-body carcinogenesis. Despite our findings and their implications, there remains no clear evidence for a direct causal connection between the surface properties of cast plates, the local CRF and the occurrence of peri-implant OSA. Nevertheless, our results add to the speculation that OSA development might be related to local surface corrosion and the influence of that condition on neighboring bone cells.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR21-757

doi: 10.3205/14dkou556, urn:nbn:de:0183-14dkou5565

Published: October 13, 2014
© 2014 Sprecher et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Biomechanischer Vergleich augmentierter und nicht-augmentierter SI-Schrauben im Hemi-Pelvis-Model

Biomechanischer Vergleich augmentierter und nicht-augmentierter SI-Schrauben im Hemi-Pelvis-Model

Grüneweller N, Raschke MJ, Widmer D, Zderic I, Wähnert D, Gueorguiev B, Fuchs T, Windolf M

Fragestellung: Die operative Versorgung von Sakruminsuffizienzfrakturen führt zu Schwierigkeiten bei der Verankerung des Osteosynthesmaterials im osteopenen Knochen. Die Zementaugmentation (ZA) von Schrauben könnte zu einer verbesserten Stabilisierung führen. Ziel dieser Studie war der paarweise biomechanische Vergleich von augmentierten (augm.) und nicht-augmentierten (n.-augm.) SI-Schrauben in einem Sakrumfrakturmodell. Speziell der klinische Versagensmodus des Herausdrehens der SI-Schraube sollte simuliert und untersucht werden.

Methodik: Zunächst wurde ein Hemi-Pelvis-Testmodell entwickelt. Mittels invers-dynamischer Analyse (AnyBody Technology, Dänemark) wurden die auf das Iliosakralgelenk wirkenden Kräfte und Momente bei normalem Gang determiniert, um eine physiologische Belastung der Iliosakral-Region trotz resezierter Symphyse sicherzustellen.

Fünf humane Beckenfrischpräparate (1 männliches, 4 weibliche, Durchschnittsalter 76,8 Jahre) wurden unter Belassen der dorsalen Bandstrukturen von sämtlichem Weichgewebe befreit. Die Symphyse wurde reseziert. Die Knochendichte des Sakralwirbelkörpers 1 wurde CT-graphisch bestimmt. Beidseitig wurde eine Sakrumosteotomie durchgeführt und mittels kanülierter SI-Schrauben (Spitze zusätzlich perforiert) stabilisiert. Randomisiert wurde je eine Schraube pro Becken mit 3 ml Knochenzement an der Schraubenspitze augmentiert.

Die biomechanische zyklische Testung erfolgte zuerst einseitig mittels biaxialer, servohydraulischer Prüfmaschine auf Grundlage der berechneten Kräfte und Momente bis zum Versagen des Konstrukts. Die andere Seite des Beckens wurde nachfolgend in identischer Weise belastet. Das Verhalten des Konstrukts wurde radiologisch und mittels optischer 3D-Bewegungsanalyse während des Tests überwacht. Als Versagenskriterien wurden Herausdrehen, Ausreißen und Auslockern der Schraube in der Frontalebene untersucht.

Die statistische Auswertung erfolgte mittels des Wilcoxon-Rangsummentests (Signifikanzniveau p<0,05).

Ergebnisse und Schlussfolgerung: Ein Herausdrehen der Schraube wurde in 50% der Tests beobachtet (3x n.-augm, 2x augm.). Durch die ZA zeigte sich ein signifikant besserer Halt der Schraube im Sakrum (p=0,043) . Das Versagen des Gesamtkonstruktes (Sakrum und Ilium) zeigte aber keinen Unterschied zwischen augm. und n.-augm. Schrauben (p=0,138). Bei den augm. Schrauben konnte in 4 Fällen ein Einbrechen der Unterlegscheibe durch die äußere Iliumkortikalis beobachtet werden.

Der Versagensmechanismus des Herausdrehens der Schraube konnte experimentell reproduziert werden. Das Modell erscheint damit valide. Die ZA verbessert zwar den Halt der Schraube im Sakrum, hat jedoch wegen vermehrten Einbrechens der Unterlegscheibe am Ilium keinen signifikanten Einfluss auf die Stabilität des Gesamtkonstruktes. Die Verwendung von größeren Unterlegscheiben könnte zu einer verbesserten Gesamtstabilität beitragen. Das Herausdrehen der Schraube konnte durch die ZA nicht durchgängig verhindert werden.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR21-1401

doi: 10.3205/14dkou555, urn:nbn:de:0183-14dkou5557

Published: October 13, 2014
© 2014 Grüneweller et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Vergleich zweier Verfahren zur Behandlung von osteoporotischen Wirbelkörperfrakturen hinsichtlich der Höhenrekonstruktion und des Höhenerhaltes im zyklischen Belastungstest

Vergleich zweier Verfahren zur Behandlung von osteoporotischen Wirbelkörperfrakturen hinsichtlich der Höhenrekonstruktion und des Höhenerhaltes im zyklischen Belastungstest

Oberkircher L, Strüwer J, Bliemel C, Bücking B, Ruchholtz S, Krüger A

Fragestellung: Die Ballon-Kyphoplastie ist ein etabliertes Verfahren zur Behandlung osteoporotischer Wirbelkörperkompressionsfrakturen. In den letzten Jahren wurden mehrere alternative Techniken im Hinblick auf die Höhenrekonstruktion entwickelt. Ziel der vorliegenden Studie war es, zwei verschiedene Methoden hinsichtlich Höhenrekonstruktion und des in einem Kadaver Modell unter zyklischer Belastung zu bewerten.

Methodik: Es wurden 25 Wirbelkörper zweier humanen Wirbelsäulen mit gesicherter Osteoporose untersucht. Nach initialer CT-Diagnostik und Entfernen der Weichteile wurden die Wirbelkörper in Technovit 3040 (Kulzer Germany) eingebettet und frakturiert. Hierzu wurde mit einer Belastungsmaschine (Instron 5566) eine axiale Last kontinuierlich gesteigert bis die Vorderkantenhöhe des Wirbelkörpers auf 30% reduziert wurde. Nach erneuter CT wurden die Wirbelkörper in einer, für Röntgenstrahlung durchlässigen Apparatur mit einer Vorlast von 100 N fixiert. 12 Wirbelkörpern wurden mittels Ballon-Kyphoplastie (Kyphon, Medtronic) und 13 Wirbelkörper mittels Radiofrequenz-Kyphoplastie (DFine, San José, CA, USA) unter der Vorlast von 100N behandelten. Anschließend erfolgte in einer servohydraulischen Belastungsmaschine (Bose Electroforce LM2 TestBench) die zyklische Belastung (100-600N, 100.000 Zyklen, 5 Hz). Danach wurde erneut eine CT durchgeführt. Anteriore, zentrale und posteriore Wirbelkörperhöhen wurden aus den jeweiligen CT-Scans für alle Zeitpunkte ermittelt.

Ergebnisse und Schlussfolgerung: Die Vorderkantenhöhe wurde nach Frakturierung 7,0 (±3) mm bei der Ballon-Kyphoplastie-Gruppe und 5,8 (±4) mm in der Radiofrequenz-Kyphoplastie-Gruppe reduziert. Statistisch gab es keinen Unterschied für die beiden Gruppen (p=1,2). Nach Augmentierung zeigte sich eine Differenz zur initialen anterioren Wirbelkörperhohe von 4,5 (±2) mm für die Ballon-Kyphoplastie-Gruppe und 4,7 (±3) mm für die Radiofrequenz-Kyphoplastie-Gruppe. Innerhalb der Gruppen gab es keinen signifikanten Unterschied (p=0,13). Nach zyklischer Belastung betrug die Differenz zur anterioren Ausgangshöhe 5,3 (±3) mm für die Ballon-Kyphoplastie-Gruppe und 5,2 (±3) mm für die Radiofrequenz-Kyphoplastie-Gruppe (p=0,2). Das durchschnittlich benötigte Zementvolumen betrug 8.7 (±1) ml für die Ballon-Kyphoplastie-Gruppe und 4.8 (±2) ml für die Radiofrequenz-Kyphoplastie-Gruppe. Der Unterschied war signifikant (p<0,0001).

Schlussfolgerung: Sowohl die bipedikuläre Ballon-Kyphoplastie als auch die unipedikuläre Radiofrequenz-Kyphoplastie resultierten in dem Kadaver Modell unter Vorlast und zyklischer Belastung in zufriedenstellender und vergleichbarer Höhenrekonstruktion sowie Höhenerhaltung ohne statistisch signifikanten Unterschied innerhalb der Gruppen. Die Radiofrequenz-Kyphoplastie benötigte signifikant geringere Mengen an Zement. Basierend auf diesen Ergebnissen könnte die Radiofrequenz-Kyphoplastie bei osteoporotischen Kompressionsfrakturen eine vielversprechende Alternative für den klinischen Bereich darstellen.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR21-1261

doi: 10.3205/14dkou554, urn:nbn:de:0183-14dkou5549

Published: October 13, 2014
© 2014 Oberkircher et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Ist die zementaugmentierte Densverschraubung der konventionellen Versorgung bei osteoporotischen Frakturen Überlegen? – Ein biomechanischer Vergleich

Ist die zementaugmentierte Densverschraubung der konventionellen Versorgung bei osteoporotischen Frakturen Überlegen? – Ein biomechanischer Vergleich

Berger-Roscher N, Waschke A, Kalff R, Wilke HJ

Fragestellung: Bei geriatrischen Patienten konnte die Osteoporose des Dens axis als ein wesentlicher Prädiktor für die Ausbildung einer Pseudarthrose nach Verschraubung von Typ-2-Densfrakturen identifiziert werden. Es ist jedoch bekannt, dass die Osteoporose einen verminderten Schraubenhalt bedingt und eine suffiziente Kompression des Frakturspaltes problematisch ist. Wir stellen daher die Hypothese auf, dass bei Vorliegen von verminderter Knochenqualität die zementaugmentierte Verschraubung der herkömmlichen Verschraubung der Densfraktur überlegen ist.

Methodik: Insgesamt wurden 18 humane Axispräparate (Median 86,5 Jahre; 69–98 Jahre) verwendet. Alle Präparate wurden auf ihre Knochenmineraldichte (BMD) hin untersucht mittels quantitativer Computertomographie in derjenigen Region, in welcher die Position des Schraubenschaftes erwartet wurde. Es wurden zwei vergleichbare Gruppen gebildet, deren mittlere Knochendichte und Alter sich nicht signifikant unterscheiden (p = 0,31 bzw. p = 0,71; Shapiro-Wilk, t-Test) (Tabelle 1 [Tab. 1]). Bei allen Präparaten wurde durch einen scharfen Meißel eine Typ-2-Fraktur erzeugt und diese durch eine neu entwickelte kanülierte und im Bereich des Axiskörpers perforierte Spezialschraube verschraubt. Bei neun Präparaten erfolgte eine zusätzliche Zementaugmentation über die Schraube mit hochviskösem PMMA-Zement. Der Sitz der Schraube und die Zementverteilung wurden durch Computertomographie überprüft. Die Stabilität der Osteosynthese wurde per Versagenstest durch Applikation einer Querkraft senkrecht auf den Dens axis getestet. Zur präzisen Verformungsanalyse wurde ein externer Laser verwendet.

Ergebnisse und Schlussfolgerung: Bei der zementierten Verschraubung war die Maximalkraft bei Versagen 2,3 fach höher (p<0,001, Mann-Whitney) und die Steifigkeit war 1,7 fach größer (p=0,039, Mann-Whitney) (Tabelle 1 [Tab. 1]). Die Zementverteilung zeigte sich in allen Präparaten zirkumferent um den Schraubenschaft ohne Auswanderung in Richtung Frakturspalt oder Spinalkanal (Abbildung 1 [Abb. 1]). Zementleckagen wurden nicht beobachtet.

Die zementierten Präparate sind den unzementierten biomechanisch statistisch deutlich überlegen in Bezug auf die Maximalkraft sowie die Steifigkeit des gesamten Konstrukts. Auf Grund der deutlich erhöhten Rigidität der Osteosynthese durch die Zementaugmentation sollte eine verbesserte Frakturheilung bei Patienten mit Osteoporose und Densfrakturen erzielbar sein. Die Technik erscheint vielversprechend im Hinblick auf die Verringerung der Pseudarthroserate nach Verschraubung von osteoporotischen Typ-2-Densfrakturen des älteren Menschen.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR21-532

doi: 10.3205/14dkou553, urn:nbn:de:0183-14dkou5531

Published: October 13, 2014
© 2014 Berger-Roscher et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Biomechanische Stabilität der zementaugmentierten anterioren Densverschraubung im in vitro-Modell

Biomechanische Stabilität der zementaugmentierten anterioren Densverschraubung im in vitro-Modell

Busse D, Schleicher P, Scholz M, Pohler K, Pingel A, Hoffmann R, Kandziora F

Fragestellung: Die Densfraktur repräsentiert bis zu 15% aller Verletzungen der HWS. Bei älteren Patienten stellt die Densfraktur die häufigste Fraktur der HWS dar. Aufgrund der Verschiebung der Alterspyramide wird eine zunehmende Häufigkeit gesehen.

Die anteriore Densverschraubung ist Standardtherapie in Fällen mit Typ II Fraktur bei jungen Patienten. Bei Osteoporose besteht das Risiko eines späteren Schraubenausbruchs mit sekundärer Frakturdislokation.

Durch Zementaugmentation konnte in der LWS die Ausrissfestigkeit eingebrachter Pedikelschrauben um 97-230% erhöht werden. Es lässt sich vermuten, dass auch die Zementaugmentation der anterioren Densverschraubung einen Stabilitätsgewinn bringt. Eine Untersuchung der Stabilität bei anteriorer Densverschraubung mit Zementaugmentation liegt bisher nicht vor, obwohl sie bereits vereinzelt im klinischen Einsatz ist.

Methodik: Untersucht wurden 14 humane HWK 2 Präparate. Sie wurden dabei nach Knochendichte in 2 Gruppen aufgeteilt. Zur Simulation der Fraktur erfolgte eine Osteotomie an der Densbasis. Nach Osteosynthese mit zwei 3,5 mm Kortikalisschrauben erfolgte in der Versuchsgruppe eine additive Zementaugmentation des Wirbelkörpers.

14 humane HWK 2 Präparate wurden in zwei Gruppen zu je 7 Präparaten aufgeteilt. In der Versuchsgruppe erfolgte nach Osteotomie an der Densbasis die direkte Verschraubung mittels zwei Kortikalisschrauben und eine zusätzliche Zementaugmentation der Densbasis. In der Vergleichsgruppe erfolgte ebensfalls eine direkte Verschraubung nach Osteotomie, jedoch keine Zementaugmentation. Das biomechanische Testprotokoll sah die Applikation einer nach posterior gerichteten Kraft an der Densvorderfläche bis zum Osteosyntheseversagen vor.

Als primär abhängige Variable wurde die Versagenslast (Fmax) erfasst. Zusätzlich wurde der Versagensmechanismus deskriptiv ermittelt. Als Kofaktor wurde die Knochendichte (BMD) in die Untersuchung mit einbezogen.

Ergebnisse und Schlussfolgerung: Die mittlere BMD lag in der Versuchsgruppe bei 273 mg/ccm, in der Kontrollgruppe bei 270 g/ccm, bei Normalverteilung in beiden Gruppen.

Die Fmax betrug in der nicht-zementierten Gruppe 729 N (+/-335 N) und in der zementierten Gruppe 745 N (+/-382 N). Der Unterschied war nicht signifikant (p=0,912).

Die BMD hatte demgegenüber einen hochsignifikanten Einfluss auf die Versagenslast (p<0,001).

Bei der Analyse des Versagensmechanismus trat in fast allen Fällen das dorsale Durchschneiden der Schrauben im Wirbelkörper auf.

Ein Vorteil der Zementierung der Denserschraubung konnte in diesem Versuch nicht nachgewiesen werden. Die Zementierung der anterioren Densosteosynthese muss dementsprechend kritisch bewertet werden.

Einschränkend ist allerdings zu erwähnen, dass das im klinischen Alltag häufig beobachtete Bild des anterioren Schraubenausrisses an der Densbasis nur in einem Versuch gesehen werden konnte, sodass die Relevanz dieses häufig verwendeten Modells für den klinischen Versagensmechanismus fraglich ist.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR21-777

doi: 10.3205/14dkou552, urn:nbn:de:0183-14dkou5524

Published: October 13, 2014
© 2014 Busse et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Biomechanische Testung zur Primärstabilität individueller Femurschaftprothesen gegenüber konventioneller Schaftprothesen

Biomechanische Testung zur Primärstabilität individueller Femurschaftprothesen gegenüber konventioneller Schaftprothesen

Götze C

Fragestellung: Die initiale Primärstabilität und der Auschluss von Mikrobewegungen des Hüftendorpothesenschaftes gegenüber dem Implantatlager sind Voraussetzungen für die Osteointegration und Langzeitstabilität zementfrei implantierter Femurschaftprothesen. Neben einer biokompatiblen Oberflächenstruktur der Prothese wird ein möglichst hoher Implantat-Knochen Kontakt gefordert. In einem biomechanischen Versuch soll der Einsatz individueller Femurschaftprothesen im Vergleich zu einer konventionellen Femurschaftprothese überprüft werden. Um den klinischen Einsatz der individuellen Femurschaftprothese zu rechtfertigen, ist eine bessere oder zumindest gleichwertige initiale Stabilität erforderlich.

Methodik: Die Testung erfolgte an einer individuell angepasste rechtwinkligen Gradschaftprothese. Als vergleichende konventionelle zementfreie Femurschaftprothese dient die Alloclassic-SL Femurschaftprothese mit distal fixierender Schaftphilosophie. 9 paarige humane Femora wurden für die biomechanische Testung verwendet. Zur Herstellung der individuellen Femurschaftprothese wurde das rechte Femur anhand von CT-Daten erfasst. Neben dem endofemoralen Markraum wurde die Antetorsion berechnet. Ziel der Planung war ein maximaler Knochen-Implantatkontakt. Nach Implantation der Endoprothesen wurden die paarigen Hüftendoprothesen einer standardisierten zyklischen Belastung von 200 bis zu 2000 Newton ausgesetzt. Lastaufnehmer distal und proximal im Implantat-Knochenübergang konnte die Mikrobewegung, Rotation und Verkippung des Implantates im endofemoralen Knochen analysieren (Messfehlerbreite ±2 µm).

Ergebnisse und Schlussfolgerung: Bei beiden Prothesentypen liegen die durchschnittlichen Mikrobewegungen deutlich unter dem kritischen Wert von 150 µm. Im Vergleich zwischen dem Standardschaft und der Individualendoprothese zeigt sich weder im Einsinkverhalten noch in der Rotation eine signifikante Abweichung (p<0,05). Während im proximalen Bereich des proximalen Femurs die Mikrobewegung der Individualendoprothese leichtgradig reduziert erscheint (p<0,05), ist die durchschnittliche Mikrobewegung im distalen Schaftbereich gegenüber der konventionellen Gradschaftprothese erhöht (p<0,05). Die Differenzen in der biomechanischen Testung sind geringfügig und nicht signifikant. Der klinische Einsatz der Individualendoprothetik bleibt unter Kenntnis der biomechanischen Testung allenfalls in der Versorgung komplexer sekundärer Coxarthrosen zu vertreten.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR20-513

doi: 10.3205/14dkou551, urn:nbn:de:0183-14dkou5511

Published: October 13, 2014
© 2014 Götze.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Wunsch und Wirklichkeit: Einschlagbedingte Positionsabweichungen bei Pressfit-Pfannen in der minimal-invasiven primären Hüftendoprothetik

Wunsch und Wirklichkeit: Einschlagbedingte Positionsabweichungen bei Pressfit-Pfannen in der minimal-invasiven primären Hüftendoprothetik

Springorum HR, Weber M, Wörner M, Baier C, Sendtner E, Grifka J, Renkawitz T

Fragestellung: Pressfit Verankerungen haben sich in der primären Hüftendoprothetik als verlässlicher Standard erwiesen. Dazu wählt der Operateur im Regelfall eine Pfanne, die im Diameter um einen Millimeter größer als die finale Fräse ist (underreaming). Theoretisch besteht dadurch beim Einschlagvorgang die Gefahr einer Verkippung und Abweichung zwischen der ursprünglich gewünschten und tatsächlich erreichten Pfannenposition. In der vorliegenden Arbeit wurden mit Hilfe der bildfreien Navigation Abweichungen zwischen der geplanten und tatsächlich erreichten Pfanneninklination (INKL) und Pfannenanteversion (AV) evaluiert und mögliche Zusammenhänge zu Pfannengröße, dem Kellgrenscore, der Schnittlänge und dem BMI analysiert.

Methodik: An insgesamt 50 Patienten erfolgte über einen minimal-invasiv anterioren (MicroHip®) Zugang mit Hilfe eines bildfreien Navigationssystems (Hip 6.0 prototype, Brainlab, Feldkirchen) die Implantation von zementfreien Hüft-Totalendoprothesen (Pinnacle, Corail, DePuy Warsaw). Zielwerte der Pfannenimplantation waren die vom Navigationssystem intraoperativ empfohlenen Werten für INKL und AV. Zu Beginn des Einschlagvorgangs positionierte der Operateur navigationskontrolliert die Pfanne in der vorgesehenen INKL und AV vor der Eingangsebene. Nach Abschluss des Einschlagvorgangs und fester pressfit-Verankerung wurde die Pfannenposition registriert und mit dem ursprünglich vorgesehenen Ausgangswert verglichen. Die statistische Beurteilung erfolgte mit deskriptiven Methoden, dem ANOVA (alpha=0,05) und dem Pearson Korrelationskoeffizienten.

Ergebnisse und Schlussfolgerung: Die mittleren Abweichungen zwischen der geplanten und der tatsächlich erreichten Pfannenposition betrug für die INKL 0,7° (±4,9°; -10° bis 14°) und für die AV 0,1° (±4,2°; -9° bis 11°). Die Berechnung des Pearson Korrelationskoeffizienten zeigte keine klinisch relevanten Zusammenhänge zwischen der Positionsabweichung der Pfanne und dem BMI des Patienten (INKL r=-0,09, AV r=0,02) oder der Schnittlänge (INKL r=-0,15, AV r=0,28). Ebenso waren weder das Arthrosestadium (INKL p=0,77, AV p=0,66) noch die Pfannengröße (INKL p=-0,43, AV p=0,17) mit dem Ausmaß der Pfannenabweichung assoziiert.

In der vorliegenden Arbeit war die Pressfit-Verankerung von Hüftpfannen in der minimal-invasiven Primärendoprothetik im Regelfall sicher möglich. Das im nordamerikanischen Sprachraum zur Vermeidung einer Fehlpositionierung gelegentlich empfohlene, vergrößerte Auffräsen des Pfannenlagers (overreaming) erscheint a priori nicht nötig. Chirurgen sollten allerdings grundsätzlich in der minimal-invasiven Hüftendoprothetik zur intraoperativen Winkelkontrolle der Pfanne auf mechanische Ausrichtinstrumente, die intraoperative Fluoroskopie oder die bildfreie Navigation zurückgreifen, um eine mögliche Fehlpositionierung nach dem Einschlagvorgang sicher auszuschließen.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR20-436

doi: 10.3205/14dkou550, urn:nbn:de:0183-14dkou5501

Published: October 13, 2014
© 2014 Springorum et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

 

Experimentelle Analyse des Deformationsverhaltens und der primären Verankerungsfestigkeit monolithischer, keramischer Hüftpfannen bei Pressfit-Verankerung

Experimentelle Analyse des Deformationsverhaltens und der primären Verankerungsfestigkeit monolithischer, keramischer Hüftpfannen bei Pressfit-Verankerung

Schulze C, Dammer R, Begand S, Oberbach T, Bader R

Fragestellung: Durch den Einsatz dünnwandiger, monolithischer Pressfit-Hüftpfannen in der Primärversorgung kann Knochenmaterial für spätere Revisionsoperationen erhalten werden. Jedoch neigen dünnwandige, künstliche Hüftpfannen beim Fixieren im Knochenlager zu Deformationen. Zu große radiale Deformationen wirken sich negativ auf den Spaltabstand (Clearance) in der Artikulationsfläche zwischen Kopf und Pfanne aus. Dadurch kann es zu erhöhtem Abrieb der Gleitpartner kommen. Eine Verformung der äußeren Pfannengeometrie begünstigt zudem Mikrobewegungen am Implantat-Knochen-Interface und verringert die Primärstabilität.Ziel dieser experimentellen Studie ist die Charakterisierung der radialen Deformation und der Verankerungsfestigkeit einer neuartigen, monolithischen Hüftpfanne aus Dispersionskeramik mit rauer und poröser Titan-Beschichtung, in Abhängigkeit von der Pressfit-Verankerung im Knochen.

Methodik: Es wurden Hüftpfannen aus ceramys® (ATZ-Keramik, Mathys Orthopädie GmbH, Mörsdorf) der Größe 44/36 und 48/40 (d.h. 44 bzw. 48 mm Außen- sowie 36 bzw. 40 mm Innendruchmesser) (jeweils n=9) untersucht. Dafür wurden Kavitäten für einen Pressfit (Unterfräsung) von 1,5/1,0/0,5 mm mittels CNC-Fräser in die PU-Schaumblöcke (Sawbones® 20 pcf, Sawbones, Malmö, Schweden) gefräst. Die Hüftpfannen wurden mittels einer servo-hydraulischen Prüfmaschine dynamisch, kraftgeregelt (F=8 kN) in die Kunstknochenblöcke eingeschlagen. Während des Einschlagvorganges wurden die tangentialen Dehnungen ε unterhalb der Pfanneneingangsebene mittels Dehnungsmessstreifen aufgenommen. Über den Ansatz ΔD=D*|ε| wurden die Durchmesseränderung ΔD berechnet. Dabei entspricht ΔD der Deformation in radialer Richtung und D dem Durchmesser der Pfannenkalotte in der Messebene (Mittelwert der Fertigungstoleranz). Zur Ermittlung der Primärstabilität wurden die Hüftpfannen anschließend weggeregelt (v=10 mm/min) aus der Knochenkavität ausgedrückt. Das erste Maximum der Ausdrückkraft Fout wurde als Maß für die Primärstabilität herangezogen.

Ergebnisse und Schlussfolgerung: Die größten radialen Deformationen wurden bei beiden Pfannengrößen entlang der Einspannungsrichtung des PU-Blocks ermittelt. Der Mittelwert der Deformation Δ D beträgt bei Pfannengröße 44/36 1,18 ± 1,03 µm und bei Pfannengröße 48/40 2,63±0,9 µm. Die Messung der Primärstabilität ergab bei Pfannengröße 44/36 Fout=345±139 N und bei Pfannengröße 48/40 Fout=372 ±157 N. Die größte Primärstabilität und die größten Deformationen wurden, bei beiden Pfannengrößen, bei einem Pressfit von 1,5 mm festgestellt.

Die radialen Deformationen verursachen eine Verringerung des Pfannendurchmessers, jedoch sind diese im Vergleich zur vorliegenden minimalen Clearance (30 µm) gering. Daraus kann eine gleichmäßige intraoperative Verklemmung der künstlichen Hüftpfannen aus ATZ-Keramik erwartet werden. Eine Unterfräsung von 1,5 mm führt, im Vergleich mit der Literatur, zu einer hohen Primärstabilität.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR20-1320

doi: 10.3205/14dkou549, urn:nbn:de:0183-14dkou5496

Published: October 13, 2014
© 2014 Schulze et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Prospektiv randomisierter Vergleich der klinischen, radiologischen und osteodensitometrischen Ergebnisse nach Implantation der zementfreien Kurzschaftprothesen Metha® und Nanos® bei primärer Koxarthrose

Prospektiv randomisierter Vergleich der klinischen, radiologischen und osteodensitometrischen Ergebnisse nach Implantation der zementfreien Kurzschaftprothesen Metha® und Nanos® bei primärer Koxarthrose

Brinkmann V, Freche S, Wohlrab D, Delank KS, Zeh A

Fragestellung: Kurzschaftprothesen haben das Ziel einer metaphysären Kraftübertragung, die ein stress-shielding des proximalen Femur verhindern und durch den Knochenerhalt eine günstigere Voraussetzung für die Revisionssituation schaffen soll.

Das Ziel der vorliegenden prospektiv randomisierten Studie bestand darin, die Migration und das Remodelling im Bereich des proximalen Femurs nach Implantation der Metha®-(Aesculap AG, Tuttlingen, Deutschland) und Nanos®-(Smith&Nephew GmbH, Marl, Deutschland) Kurzschaftprothese zu analysieren.

Methodik: Vom 01.01.2011 – 02.04.2013 wurde bei 24 Patienten (12 Frauen , 12 Männer) ein Metha®-Stem und bei 26 Patienten (10 Frauen , 16 Männer) mit primärer Koxarthrose ein Nanos®-Stem randomisiert implantiert.

Neben der radiologisch digitalen Auswertung des Stemverhaltens in Bezug auf die Migration, Varus-Valgus-Ausrichtung, Veränderung des Offsets, Center of Rotation (COR), Caput-Collum-Diaphysen-Winkels (CCD) sowie einer Beinlängenbeeinflussung, wurde das Auftreten radiotransluzenter Linien (RL) analysiert und bewertet. Darüber hinaus wurde eine gruenzonendefinierte DEXA-Untersuchung des proximalen Femurs direkt postoperativ, sowie im Durchschnitt nach ca. 3 und 12 Monaten durchgeführt. Die klinische Beurteilung erfolgte anhand der visuell analogen Schmerzskala (VAS) und dem Harris-Hip-Score (HHS).

Ergebnisse und Schlussfolgerung: Zusammengefasst ließ sich anhand der DEXA-Analyse nach 12 Monaten eine geringe aber signifikante Abnahme der BMD (Bone Mineral Density) für den Metha®-Stem in den Gruen-Zonen 1, 6 und 7, sowie für den Nanos®-Stem in den Gruen-Zonen 1 und 7 analysieren (gepaarter t-Test; p< 0,05).

Für die radiologischen Parameter Migration, Varus-Valgus-Ausrichtung, Offset, COR, CCD-Winkel und Beeinflussung der Beinlänge konnte innerhalb beider Gruppen sowie im direkten Gruppenvergleich keine statistische Signifikanz festgestellt werden (t-Test; p >0,05). Die Analyse des Auftretens von RL erbrachte keine statistisch signifikanten Unterschiede beider Prothesenstems.

Für beide Patientengruppen wurde eine statistisch signifikante Verbesserung der VAS (Mittelwert 0,7) und des HHS (Mittelwert 96 Punkte) beobachtet (gepaarter t-Test; p<0,001).

Mit beiden untersuchten Kurzschaftprothesensystemen konnten hervorragende klinische Ergebnisse erzielt werden. Beide Implantate zeigten keine Anzeichen für eine Beeinträchtigung der Osseointegration.

Ein gering ausgeprägtes stress-shielding im proximalen Femur konnte aber für beide Stems nach 12 Monaten nachgewiesen werden.

Im Vergleich zu konventionellen Femurprothesen ist die Abnahme der BMD im Bereich des proximalen Femurs als gering einzustufen, so dass für beide Prothesensysteme eine Verringerung des proximalen stress-shieldings und ein weitgehender Knochenerhalt im Vergleich zu konventionellen Stems konstatiert wird.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR20-650

doi: 10.3205/14dkou548, urn:nbn:de:0183-14dkou5484

Published: October 13, 2014
© 2014 Brinkmann et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.

Sind die mit einem Kniesimulator erzeugten Verschleißmuster vergleichbar mit der In-vivo-Situation?

Sind die mit einem Kniesimulator erzeugten Verschleißmuster vergleichbar mit der In-vivo-Situation?

Müller U, Jäger S, Reinders J, Sonntag R, Kretzer JP

Fragestellung: Die Untersuchungen des Verschleißverhaltens von künstlichen Kniegelenken im Rahmen von präklinischen Tests werden am häufigsten mit standardisierten Verschleißsimulatoren durchgeführt. Jedoch wird die Vergleichbarkeit dieser Tests zu den klinischen Beobachtungen hinsichtlich Verschleißmuster und Verschleißerscheinungen kontrovers diskutiert.

Ziel dieser Studie war es daher, zu untersuchen, ob die Fläche und die Ausdehnung der Verschleißzonen von explantierten Knieendoprothesen-Inlays vergleichbar sind mit denen, die im Verschleißsimulator erzeugt wurden.

Methodik: Für die Untersuchung standen drei Gruppen von PE-Inlays zur Verfügung. Gruppe A bestand aus 12 explantierten PE-Inlays, die an der Klinik XXX ausgebaut wurden. Zwei weitere Gruppen von PE-Inlays wurden einer Verschleißsimulation unterzogen. Bei Gruppe B wurde eine kraftgeregelte Verschleißtestung gemäß ISO 14243-1 durchgeführt. Demgegenüber erfolgte die Verschleißsimulation bei der Gruppe C weggeregelt (ISO 14243-3). Zur Verdeutlichung ihrer Position und ihrer Ausdehnung wurden die jeweiligen Verschleißzonen der medialen und lateralen Artikulationsfläche der PE-Inlays mit einem schwarzen Marker umrandet und fotografisch dokumentiert. Anschließend wurden diese mit Hilfe eines Bildbearbeitungsprogramms vermessen (Abbildung 1 [Abb. 1]).

Ergebnisse und Schlussfolgerung: Obwohl die Varianz bei den explantierten PE-Inlays wesentlich größer war, sind die Verschleißflächen auf der medialen und lateralen Artikulationsseite signifikant größer, verglichen zu denen von kraft- oder weggeregelter Verschleißsimulation. Die Ausdehnung der Verschleißzonen in AP-Richtung war bei den Explantaten größer als bei beiden Simulator-Gruppen. Jedoch besteht ein signifikanter Unterschied nur zwischen der Explantat-Gruppe und der Gruppe, bei der die Verschleißtestung weggeregelt erfolgte.

Die Fläche und die Ausdehnung der Verschleißzonen in AP- und ML-Richtung ist geringer bei den Inlays der beiden Simulator-Gruppen verglichen zu den Explantaten. Allerdings scheint es so, dass die kraftgeregelte Verschleißtestung zu ähnlicheren Verschleißmustern führt als die weggeregelte Testung.

Folglich sind Knieverschleißsimulatoren nicht vollständig in der Lage, die komplexen In-vivo-Kinematiken und -Belastungen nachzuahmen und können daher nicht alle möglichen Verschleißmuster, die bei Explantaten beobachtet werden, abbilden.

Zukünftig sollte daher das Ziel sein, die Verschleißtestung von Knieendoprothesen unter Verwendung von höheren Belastungsprofilen oder abwechslungsreicheren Aktivitätsprofilen zu verbessern.

 

Deutscher Kongress für Orthopädie und Unfallchirurgie (DKOU 2014). Berlin, 28.-31.10.2014. Düsseldorf: German Medical Science GMS Publishing House; 2014. DocGR20-1035

doi: 10.3205/14dkou547, urn:nbn:de:0183-14dkou5476

Published: October 13, 2014
© 2014 Müller et al.
This is an Open Access article distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by-nc-nd/3.0/deed.en). You are free: to Share – to copy, distribute and transmit the work, provided the original author and source are credited.